STEP 04 · 热压 / 养生
LVL Hot Pressing & Conditioning The assembled veneer panels are hot-pressed under controlled temperature, pressure and time to ensure proper phenolic adhesive curing and strong layer bonding. After pressing, panels undergo spacer-assisted cooling and conditioning, followed by thickness inspection to ensure dimensional accuracy and consistent structural quality.
Explore YELU WOOD's structural LVL hot pressing and conditioning process. Our 6.6-meter hydraulic hot press operates at controlled temperatures of 140–160°C and pressures of 1.2–1.6 MPa. From phenolic adhesive curing and panel consolidation to spacer-assisted cooling and multi-point thickness inspection, every stage is carefully controlled to ensure consistent bonding, dimensional stability and reliable structural performance.